IME IZDELKA: EPOKSIDIZIRANA SOJINSKA OLJA
MANUFATURER: ZHEJIANG JIAAO ENPROTECH STOCK CO LTD
ŠTEVILKA SERIJE: 201703002
TOČKE | STANDARD | REZULTAT |
EPOXY VALUE (%) ASTMD1652-04 | 6.6MIN | 6.71 |
COLOR SHADE (pt-co) | 1 50 MAX | 145 |
GOSTOTA (20 ℃ g / cm3 ) | 0,988-0,998 | 0,9885 |
IODINA VALUE (%) | 5 .0MAX | 1.50 |
KISLINA VREDNOST (mg KOH / g) | 0.6MAX | 0,40 |
VSEBNOST VLAGE(%) | 0.3MAX | 0.05 |
FLASH TOČKA (℃) | 280MIN | 301 |
ZAKLJUČEK | SPREJEMO | |